Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Journal
Article Type
Date
Availability
1-1 of 1
D.N. Leonard
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Cast Alumina-Forming Austenitic Stainless Steels for High Temperature Heat Treatment Furnace Rolls
Available to Purchase
Journal: AM&P Technical Articles
AM&P Technical Articles (2024) 182 (4): 46–49.
Published: 01 May 2024
Abstract
View articletitled, Cast Alumina-Forming Austenitic Stainless Steels for High Temperature Heat Treatment Furnace Rolls
View
PDF
for article titled, Cast Alumina-Forming Austenitic Stainless Steels for High Temperature Heat Treatment Furnace Rolls
Alloy developers worldwide have struggled to create creep-resistant alumina-forming, iron-based austenitic stainless steels for use as high-temperature structural alloys, but with limited success in balancing alloy cost, oxidation, and creep resistance. This article describes the research and development of a novel cast alumina-forming austenitic stainless steel. This work won the prestigious Engineering Materials Achievement Award presented at IMAT 2023 in Detroit.