Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Article Type
Volume Subject Area
Date
Availability
1-1 of 1
Axelle Elrikh
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Proceedings Papers
Improving the Adhesion of Wear-Resistant Coatings on Aerospace Polymer Composites
Available to Purchase
ITSC 2015, Thermal Spray 2015: Proceedings from the International Thermal Spray Conference, 87-91, May 11–14, 2015,
Abstract
View Papertitled, Improving the Adhesion of Wear-Resistant Coatings on Aerospace Polymer Composites
View
PDF
for content titled, Improving the Adhesion of Wear-Resistant Coatings on Aerospace Polymer Composites
Fiber-reinforced polymer composites (CFRP) are increasingly used in aerospace for weight-sensitive applications. However, they are subjected to degradation from the erosive forces of solid particles and water droplets. This degradation results in a decreased service life of composite components and increased repair costs. A coating can protect the CFRP surface against wear and plasma spraying could be a candidate technique to achieve this coating. However, an issue is the thermal and mechanical damage to the composite surface by the plasma-sprayed particles. Another issue is the coating adhesion, because of the low wettability of polymer surface to liquid metal and ceramic and different atomistic properties between substrate and coating material. A possible solution to both issues is the use of a primary layer deposited by a “softer” technique than thermal spraying. This study deals with the deposition of this primary layer by three methods (magnetron sputtering, air gun spraying and sol-gel) and the deposition of topcoat layer by plasma spraying. The effectiveness of the protection of the CRFP by the primary layer during topcoat plasma spraying is investigated as well as the interfaces of the duplex coatings.