Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Subjects
Article Type
Date
Availability
1-1 of 1
Amanda Leong
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Proceedings Papers
AM-EPRI2024, Advances in Materials, Manufacturing, and Repair for Power Plants: Proceedings from the Tenth International Conference, 1331-1337, October 15–18, 2024,
Abstract
View Paper
PDF
A thorough understanding of interactions between graphite and fluoride fuel salts is crucial, as graphite is a promising candidate for the moderator of molten salt reactors. This study investigates the infiltration of fluoride fuel salts into graphite and the fluorination of graphite by these salts under various pressures and temperatures. A high-pressure salt infiltration test apparatus was developed to examine the infiltration of NaF-KF-UF 4 and NaF-BeF 2 -UF 4 -ZrF 4 fuel salts into two types of graphite at high temperatures. For tests using NaF-BeF 2 -UF 4 -ZrF 4 , two different temperatures were selected to assess the impact of temperature on threshold pressure. The study observed salt infiltration into graphite at pressures exceeding its threshold pressure, and the threshold pressure for infiltration was lower at the higher temperature. In addition, the formation of carbon fluorides on the surface of post-test graphite specimens was identified.