Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Article Type
Volume Subject Area
Date
Availability
1-1 of 1
Alfonso Fuentes-Aznar
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Proceedings Papers
HT2023, Heat Treat 2023: Proceedings from the 32nd Heat Treating Society Conference and Exposition, 142-149, October 17–19, 2023,
Abstract
View Papertitled, Integrated Heat-Treatment Simulation with Virtual Inspection of Distorted Gears
View
PDF
for content titled, Integrated Heat-Treatment Simulation with Virtual Inspection of Distorted Gears
Heat-treatment simulation is a powerful tool for gear design and process troubleshooting, but many times the predicted gear distortion is difficult to compare to physical gear measurements and to required specification charts or measurements. To help ease this burden, two software programs are utilized to provide powerful gear analyses to heat-treatment simulation results. This paper briefly describes the software used, DANTE and Integrated Gear Design (IGD), and presents a simple case study. The stress and deformation from the heat treatment of a small gear made of SAE 10B22 are predicted using DANTE. The distorted gear geometry is then imported into IGD and the predicted distortion is compared to the actual measurements of the gear.