ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 167-170, May 24–28, 2021,
...Abstract Abstract Light water reactors (LWR) use zirconium-alloy fuel claddings, the tubes that hold the uranium-dioxide fuel pellets. Zr-alloys have very good neutron transparency, but during a loss of coolant accident or beyond design basis accident (BDBA) they can undergo excessive oxidation...
Proceedings Papers

ITSC2000, Thermal Spray 2000: Proceedings from the International Thermal Spray Conference, 999-1004, May 8–11, 2000,
...Abstract Abstract Borides are promising materials with good wear and corrosion resistance properties. Boride coatings are expected to perform better where wear and corrosion resistances are simultaneously required. Zirconium diboride is an important emerging material for such applications, due...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 623-626, May 24–28, 2021,
... velocities and the ensuing, through plastic stainless steel canisters that house the UNF (consisting of deformation and associated adiabatic shear at the interfaces of zirconium-alloy fuel cladding tubes with used uranium-dioxide the particles and particles and substrate result in the formation fuel...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 422-430, May 24–28, 2021,
... the in many industrial applications because of its high deposition Seebeck coefficient, the electrical conductivity, the total rate (4kg/h), its high flexibility in terms of sprayable materials thermal conductivity, and T the absolute temperature in Kelvin (metals, complex multi-component alloys, ceramics...
Proceedings Papers

ITSC 2002, Thermal Spray 2002: Proceedings from the International Thermal Spray Conference, 788-792, March 4–6, 2002,
...Abstract Abstract This paper consists of laws of formation of the modified layer on a surface of coatings from zirconium dioxide with the help of laser radiation. The peculiarities of laser processing of TSZ plasma sprayed layers on steel substrates with NiCrAlY bond layers are investigated...
Proceedings Papers

ITSC1996, Thermal Spray 1996: Proceedings from the National Thermal Spray Conference, 65-72, October 7–11, 1996,
... of the use of thick (up to 5 mm) stainless steel or bronze coatings as claddings on steel, aluminum or zirconium rods in order to provide good ultrasonic wave guides are given. Compared to a conventional non-clad rod the signal to noise ratio of such clad rods has been improved by more than 40 dB due...
Proceedings Papers

ITSC 2002, Thermal Spray 2002: Proceedings from the International Thermal Spray Conference, 755-759, March 4–6, 2002,
... stabilized zirconia thermal insulation layers based on zirconium oxide. 22 magnesium oxide-zirconium dioxide thermal barrier coatings are sealed with normal orthophosphoric acid. The microstructure of thermal barrier coatings based on zirconium oxide is extensively investigated. In yttria stabilized zirconia...
Proceedings Papers

ITSC 2002, Thermal Spray 2002: Proceedings from the International Thermal Spray Conference, 335-338, March 4–6, 2002,
... for the possibility to produce from their sizes (20-100 µm) is low. coatings from metals (aluminium, copper, nickel, titanium, molybdenum etc aluminium, copper, References iron, nickel, cobalt alloys; aluminium, zirconium and titanium oxides; tungsten carbide, bioceram- 1. Yuschenko K., Borisov Yu., Pereverzev Yu. et...
Proceedings Papers

ITSC1996, Thermal Spray 1996: Proceedings from the National Thermal Spray Conference, 897-904, October 7–11, 1996,
... of the bond coat. The bond coat, an alloy of alloy, is to increase durability of the TBC by protecting the NiCoCrAlY was sprayed in 6 layers to a 0.12 mm base material fi'om corrosion and oxidation, and by thickness, and the ceramic top coat, yttrium stabilised promoting the adherence of the top coat...
Proceedings Papers

ITSC1996, Thermal Spray 1996: Proceedings from the National Thermal Spray Conference, 477-482, October 7–11, 1996,
... techniques, including post-spray alumina (Dispal 23N4-20, Vista Chemical Co., Houston, TX), zirconia (zirconium butoxide in n- sealing, high temperature heat treatment, hot butanol, Aldridge, WI) and YSZ (zirconium and isostatic pressing and laser/particle beam glazing, yttrium acetates dissolved in dilute...
Proceedings Papers

ITSC 2002, Thermal Spray 2002: Proceedings from the International Thermal Spray Conference, 721-726, March 4–6, 2002,
...Abstract Abstract This paper deals with experimental and theoretical aspects of the post-treatment of thermally sprayed layers with high-power lasers. Various layers, such as VPS-sprayed CoCrAlY layers, APS-sprayed zirconium dioxide, aluminum oxide, and hydroxyapatite layers, as well as APS...
Proceedings Papers

ITSC 2002, Thermal Spray 2002: Proceedings from the International Thermal Spray Conference, 6-11, March 4–6, 2002,
..., 11]. coatings from oxides of aluminium, zirconium and be- ryllium. They feature the purely diffuse reflection within the wide range of the wavelengths (0.2-3 mi- crons), this making them superior in this respect to other types of the coatings, such as paintwork or vac- uum coatings. The positive...
Proceedings Papers

ITSC 2002, Thermal Spray 2002: Proceedings from the International Thermal Spray Conference, 231-235, March 4–6, 2002,
... are zirconium oxides stabilized by means of yttrium oxide or other types of stabilization. This article describes the developments in the named areas that lead to an improvement in both the technical behavior and the commercial boundary conditions. Novel types of spray additives as well as novel and further...
Proceedings Papers

ITSC 2002, Thermal Spray 2002: Proceedings from the International Thermal Spray Conference, 765-770, March 4–6, 2002,
...Abstract Abstract A 3D model for heat transfer and stress evaluation during plasma spraying was developed for MSC/MARC. The substrate-layer system is represented by a sheet metal (strip) with the dimensions 120x20x2 mm and a zirconium dioxide+7% yttrium oxide layer with a thickness of 0.06 mm...
Proceedings Papers

ITSC 2002, Thermal Spray 2002: Proceedings from the International Thermal Spray Conference, 324-329, March 4–6, 2002,
... shape. The theoretical analyzes and the mathematical models are confirmed by means of X-ray examinations. The investigations are carried out using the sin square Psi technique on conical yttria partially stabilized zirconium oxide samples with various clamping mandrel removal methods; the measurements...
Proceedings Papers

ITSC1998, Thermal Spray 1998: Proceedings from the International Thermal Spray Conference, 1271-1276, May 25–29, 1998,
...) to aid in densification and - 10wf% tungsten and niobium - 1.0wt% zirconium. the reduction of oxides. Both a liquid phase sinter Only the Nb-lZr material was a truly alloyed powder, (LPS) and a solid state sinter (SSS) were used on the all of the other compositions were comprised of W-Ni-Fe alloy...
Proceedings Papers

ITSC1997, Thermal Spray 1997: Proceedings from the United Thermal Spray Conference, 757-762, September 15–18, 1997,
...Abstract Abstract A technique has been developed to characterize the elastic modulus of zirconium oxide - 8 % yttrium oxide plasma sprayed deposits. A commercial hardness indenter has been modified to record load - displacement as a spherical ball is elastically loaded onto the surface...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 447-453, May 24–28, 2021,
... Coating, J. Alloys Comp., 765, 1082-1089 (2018). [11] H. Sun and R.D. Pehlke, Modeling and Experimental Study of Gaseous Oxidation of Liquid Iron Alloys, [2] R.-G. Xie , D. Li, G.-J. Yang and C.-J. Li, The Influence Metall. Mater. Trans. B., 27, 854-864 (1996). of Zirconium Carbide Addition...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 31-35, May 24–28, 2021,
... temperature capability and improve the reliability of abradable seal structures. A cavity layer of honeycomb seal structure made of SS 321 alloy was coated with advanced high-temperature ZrO 2 +7.5%Y 2 O 3 +4% polyester seal material using TriplexPro-210 plasma spray system. The integrity of a seal structure...
Proceedings Papers

ITSC1998, Thermal Spray 1998: Proceedings from the International Thermal Spray Conference, 103-109, May 25–29, 1998,
... life 104 particles transferred during wear were smaller for the significantly reduce both the general and galvanic plasma sprayed alloys than for the wrought because of the corrosion of a coating. lamellar nature of the coatings. The electroplated coatings such as chromium are Erosive wear is caused...