1-8 of 8 Search Results for

twinning-induced plasticity steel

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 278-282, May 24–28, 2021,
... modern steel grades such as TWIP (twinning-induced plasticity steel). In this study, a (Ti,Mo)(C,N)-29% Ni hardmetal feedstock powder was prepared by agglomeration and sintering. Coatings were deposited using a high velocity air-fuel (HVAF) spray process. The coating was benchmarked against a standard...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 750-757, May 24–28, 2021,
...: Composition of the feedstock material on C45 steel specimens using twin wire arc spraying (TWAS) [13]. However, the induced stresses and obtained hardnesses are For the coating process, dry and compressed air was utilized as inhomogeneous and depend directly on the peening direction. an atomization gas...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 177-188, May 24–28, 2021,
... when hitting a substrate. They undergo intense and Cold spray coatings studied in this paper were elaborated with extremely fast plastic deformation during the impact, as well a commercial austenitic stainless steel 316L powder (see as during coating build-up. Impacts lead to mechanical and composition...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 290-297, May 24–28, 2021,
... the Martensitic Transformation in AISI 304 Steel Sheets Processes," Wear, Vol. 394 395, (2018), p 113 133. Subjected to Tension under Wide Ranges of Strain Rate at httpsdoi.org/10.1016/j.wear.2017.10.014. 21. M. Bayerlein, et al., "Plasticity-Induced Martensitic Room Temperature," Mater. Sci. Eng. A, Vol. 528...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 530-541, May 24–28, 2021,
... Abstract Twin wire arc is a commonly used thermal spray technology for application of steel coatings to cast iron components. Hardness and adhesion strength are critical properties of such coatings, and significant research is available reporting these properties. However, residual stresses...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 527-529, May 24–28, 2021,
...], and Inconel [6] onto a similar family of substrate metals. During the coating operation, there are five Twin wire arc is a commonly used thermal spray technology for key processing parameters that can be modified to change the application of steel coatings to cast iron components. Hardness properties...
Proceedings Papers

ITSC2000, Thermal Spray 2000: Proceedings from the International Thermal Spray Conference, 423-428, May 8–11, 2000,
... m resulting from the stainless steel of the same composition. Additional coupons of residual stresses induced by coating a polished coupon of the A36 carbon steel were also coated and examined, as described stainless steel with a Ni-Al bond coat and a 1 mm thick spinel below. layer. The stainless...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 431-439, May 24–28, 2021,
... Abstract FeMnCrSi alloys have been developed and studied over the past several years with an emphasis on their use as coatings on CA6NM stainless steel hydroturbine components. Much of the work conducted has focused on the optimization of cavitation resistance through chemical composition...