ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 96-100, May 24–28, 2021,
... solutions which enable these industries to increase their productivity and level of manufacturing quality. silicone masking thermal spraying Thermal Spray 2021: Proceedings from the International Thermal Spray Conference Copyright © 2021 ASM International® May 24 28, 2021 All rights reserved. F...
Proceedings Papers

ITSC 2002, Thermal Spray 2002: Proceedings from the International Thermal Spray Conference, 390-396, March 4–6, 2002,
... removal. plasma coatings. A thin plasma-sprayed nickel- The remaining grinding steps were conducted with aluminum and a thick arc-sprayed silicon bronze rigid diamond grinding discs, fixed diamond films, or were chosen to represent soft and porous coatings. diamond suspensions on hard napless cloths. Fine...
Proceedings Papers

ITSC1997, Thermal Spray 1997: Proceedings from the United Thermal Spray Conference, 11-19, September 15–18, 1997,
... spray process for the coating of aluminum-silicon cylinder block bores using a rotating plasma gun capable of producing coatings of reliable microstructure and integrity. Properties and microstructures of the applied coatings will be presented. Test results will be shown that the necessary bond strength...
Proceedings Papers

ITSC1998, Thermal Spray 1998: Proceedings from the International Thermal Spray Conference, 963-974, May 25–29, 1998,
... spray process for the coating of aluminum-silicon cylinder block bores using a rotating plasma gun capable of producing coatings of reliable microstructure and integrity. Properties and microstructures of the applied coatings will be presented. Test results will be shown that the necessary bond strength...
Proceedings Papers

ITSC1998, Thermal Spray 1998: Proceedings from the International Thermal Spray Conference, 659-664, May 25–29, 1998,
..., while large pit corrosionis developed induction furnace. A small amount of silicon was added to in a SUS316L stainlesssteel sheet. prevent oxidationthrough atomization. Alloy powders under 45/.l m diameter were used for spraying. Coatings of about THE AUTHORS have investigated formation and tempering...
Proceedings Papers

ITSC1998, Thermal Spray 1998: Proceedings from the International Thermal Spray Conference, 43-48, May 25–29, 1998,
... was determined in 3.5 wt% LSA-6 NaCI in orderto simulatemarineenvironment. LSA-7 3 1250 0.5 x6.0 LSA-8 ExperilDeDtal~ethods LSA-9 1 750 0.5 x6.0 The samples of size 1Oem x 10cm x 0.4cm thick 2 750 0.5 x 6.0 were cut from SS 304 sheet. These were polished with 320 and 600 grit silicon carbide 4 750 0.5 x 6.0...
Proceedings Papers

ITSC2000, Thermal Spray 2000: Proceedings from the International Thermal Spray Conference, 1025-1031, May 8–11, 2000,
... substrate. The galvanic corrosion is derived from the difference of corrosion potential between two materials. In the 1025 present stage, the elimination of the porosity or SiC paper up to # 600, rinsed with acetone, and penetration in the thermally sprayed coating is more completely masked with silicone...
Proceedings Papers

ITSC2000, Thermal Spray 2000: Proceedings from the International Thermal Spray Conference, 471-478, May 8–11, 2000,
... elemental loss of chromium, carbon, agglomerated and sintered tungsten carbide - 17wt% cobalt (A- boron and silicon in self-fluxing alloys, carbide cermets, and 17). Table 1 summarizes the main characteristic of these corrosion resistant alloys during the spray process (1). Hybrid powders including...