ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 167-170, May 24–28, 2021,
... and steam environments at temperatures in excess of 1100 °C, while maintaining excellent adhesion to the substrate. These and other results of this study, including mechanical property evaluations, will be presented. chromium coatings cold spraying nuclear fuel cladding oxidation resistance...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 623-626, May 24–28, 2021,
...Abstract Abstract Cold spray deposition is being investigated for mitigation of chloride-induced stress corrosion cracking (CISCC) in dry cask storage systems (DCSS) for spent nuclear fuel. Welded regions of austenitic stainless-steel canisters in DCSS are under tensile stress and susceptible...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 307-314, May 24–28, 2021,
... wrought FeCrAl fuel cladding (2013), p 495-505. doi:10.1007/s11085-012-9338-y for light water reactors," Journal of Nuclear Materials, Vol. 467 (2015), p 703-716, 2015. [24] H. Buscail, et al, "Water vapour effect on the oxidation doi:10.1016/j.jnucmat.2015.10.019 mechanism of a cobalt-based alloy at high...