ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 331-339, May 24–28, 2021,
.... In this study, a post-spray sealing treatment of Cr3C2-NiCr/Al2O3-TiO2 plasma sprayed coatings was carried out, then their corrosion properties were evaluated, before and after the treatment. For sealing process, aluminum phosphate (APP) containing aluminum oxide (Al2O3) nanoparticles (~10 nm) was used...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 461-472, May 24–28, 2021,
..., straight pipe runs. filtration systems nanoparticles operator safety particle exposure plasma spraying equipment Thermal Spray 2021: Proceedings from the International Thermal Spray Conference Copyright © 2021 ASM International® May 24 28, 2021 All rights reserved. F. Azarmi, X. Chen, J. Cizek...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 354-359, May 24–28, 2021,
... Abstract Up to now, the role of particle sizes on deformation features of ceramic particles in aerosol deposition (AD), is not fully understood. For distinguishing general features, two-dimensional molecular dynamics (MD) simulations are applied to study associated phenomena. The nanoparticles...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 635-647, May 24–28, 2021,
... Abstract This paper addresses a need for information on nanoparticle emissions and related issues such as worker exposure, filtration efficiency, and dustiness. A survey has been conducted on the working conditions and safety measures used in thermal spray companies and the results compared...
Proceedings Papers

ITSC2000, Thermal Spray 2000: Proceedings from the International Thermal Spray Conference, 971-976, May 8–11, 2000,
... (pyrolysis, reduction and carburization) of that coatings, recent efforts have been directed at using powder to form the desired nanophase WC/Co end- nanoparticle agglomerates as feed materials. However, the product powder. Multimodal WC/Co powder is produced enhanced properties that were observed...
Proceedings Papers

ITSC1997, Thermal Spray 1997: Proceedings from the United Thermal Spray Conference, 877-883, September 15–18, 1997,
... processing is a potential solution reinforcement. The latest results of process- for overcoming the processing limitations of structure-property relationship studies in silica nanoparticle reinforced polymer composites. The and carbon black reinforced nylon 11 coatings are need for volatile organic solvents...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 340-345, May 24–28, 2021,
..., J. Quirk and K. Masenelli-Varlot, Mechanical behavior law of ceramic nanoparticles from transmission electron microscopy in situ nano-compression tests, Materials Letters, 119, 2014, 107-110. [8] A. Elsenberg, F. Gärtner, T. Klassen, Aerosol Deposition of Ti3SiC2-MAX-Phase coatings, Journal...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 578-584, May 24–28, 2021,
....; Boccaccini, A.R. Surface & Coatings Technology Development of bioactive review. World J. Clin. Cases 2015, 3, 52, composite coatings based on combination of PEEK , bioactive glass and Ag nanoparticles with antibacterial doi:10.12998/wjcc.v3.i1.52. properties. Surf. Coat. Technol. 2016, 301, 100 105, doi...
Proceedings Papers

ITSC1997, Thermal Spray 1997: Proceedings from the United Thermal Spray Conference, 543-548, September 15–18, 1997,
... loss from vaporization has been studied by addressing the change in particle size after passage in the plasma but more recently by studying the vaporization within the plasma [3-5]. A third approach entails collection of nanoparticles from the vapor formed in the plasma. 543 particles are deflected...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 585-589, May 24–28, 2021,
... of bacteria and caused the death of bacteria. serially diluted 10 times using 10 fold. After that 5 µL of the Moreover, titania was more effective in the form of each diluted suspension was spotted on agar medium and nanoparticle. Homogeneous distribution of fine particles in incubated at 370 C for 18 h...
Proceedings Papers

ITSC1997, Thermal Spray 1997: Proceedings from the United Thermal Spray Conference, 329-333, September 15–18, 1997,
... is suitable for depositing particles in the 10 nm size range. The deposited materials were analyzed using electron microscopy and X-ray diffraction. For the silicon runs, the plasma conditions upstream of the nozzle were similar to those used in our previous work on silicon nanoparticle synthesis...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 235-240, May 24–28, 2021,
... of a nanoparticle onto a substrate [1]. Metallurgical bonding involves the formation of substrate. Despite the valuable physical information which MD atomic bonds (chemical bond) between the particle and the simulations provide about the whole adhesion process, the substrate. This type of bonding requires that two...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 322-330, May 24–28, 2021,
...., Effects of aluminum phosphate heat treatments on corrosion behavior of plasma sprayed containing Al2O3 nanoparticles on the hardness and wear Cr2O3-Al2O3 composite ceramic coatings, Surface & resistance of the Al2O3-TiO2 plasma sprayed coating, Coatings Tech, Vol. 276 (2015), p 8 15. doi: Vietnam J...
Proceedings Papers

ITSC2000, Thermal Spray 2000: Proceedings from the International Thermal Spray Conference, 919-928, May 8–11, 2000,
... is the quenching close to the whole TPCVD process of SiC can be proposed, see Fig. 25. substrate surface, the smaller are the agglomerates. The volume of the reactor separating the substrate from the Agglomeration or coalescence of nanoparticles is easier far disilane precursor injection point can be divided...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 473-481, May 24–28, 2021,
..., Nano Lett., Vol. 20, No. 12, p 8508 8515, doi: 10.1021/acs.nanolett.0c02956. P. Juuti, et al., Achieving a slippery, liquid-infused porous surface with anti-icing properties by direct deposition of flame synthesized aerosol nanoparticles on a thermally fragile substrate, Appl. Phys. Lett., Vol. 110...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 527-529, May 24–28, 2021,
... coatings Optimized part features and dimensions to reduce Less overspray overall mass. Lower defect rate More effective spraying of nanoparticles in Larger gas jet lines to reduce back pressure. Integrated features to reduce the total number of suspension parts. 527 Multi-start threaded...