Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 171-176, May 24–28, 2021,
... treatment was studied and correlated with their deformation behavior during the cold spray deposition. Deposits sprayed with heat-treated powders at 800 and 900 °C and nitrogen showed less particle deformation and higher porosity as compared to as-atomized deposit associated to the presence of delta phase...
Proceedings Papers

ITSC2000, Thermal Spray 2000: Proceedings from the International Thermal Spray Conference, 905-908, May 8–11, 2000,
... Abstract Layers of high-purity copper and iron produced by cold gas-dynamic spraying have been thermally processed to induce recrystallization and grain growth. In the case of copper deposits, the as-sprayed structure could be "pinned" by arrays of Cu2O particles present on the surfaces...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 247-255, May 24–28, 2021,
... Abstract In this study, a novel strategy to manufacture high strength cold-sprayed Al coating by using powder with wide size distribution is proposed. The microstructure and mechanical properties of deposited coating sprayed at three typical impact velocities before and after heat treatment...
Proceedings Papers

ITSC1997, Thermal Spray 1997: Proceedings from the United Thermal Spray Conference, 361-367, September 15–18, 1997,
... www.asminternational.org DOI: 10.31399/asm.cp.itsc1997p0361 Thermal Spray: A United Forum for Scientific and Technological Advances, C.C. Bemdt(Ed Published by ASM International, Materials Park, Ohio, USA, 1997 Deposition of Nickel-Aluminum Bronze Powder by Cold Gas-Dynamic Spray Method on 2618 Al for Developing Wear...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 241-246, May 24–28, 2021,
... configurations. Thus, window of deposition was increased with laser surface texturing. Anchoring mechanisms increased two fold the adhesion strength compared to conventional pre-treatments. In one case, the interface was stronger than the coating cohesive strength. adhesion bond strength cold spraying...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 51-59, May 24–28, 2021,
... of different processing sequences on MCrAlY coating characteristics and short-term isothermal oxidation performance were investigated. Specifically, cold spray deposition of NiCoCrAlTaY coatings was carried out on single-crystal Ni-base superalloy substrates that underwent various degrees of the full heat...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 87-95, May 24–28, 2021,
.... The development of an automated technology to metallize polymer based composite for lightning strike protection is the aim of the CO3 project (EU Grant agreement: ID831979). In this study, thermal and electrical conductivities of composites were achieved by cold spray deposition of Cu or Al coatings. Critical...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 623-626, May 24–28, 2021,
... Abstract Cold spray deposition is being investigated for mitigation of chloride-induced stress corrosion cracking (CISCC) in dry cask storage systems (DCSS) for spent nuclear fuel. Welded regions of austenitic stainless-steel canisters in DCSS are under tensile stress and susceptible...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 611-615, May 24–28, 2021,
... Abstract A previous study showed that Cu can be cold sprayed onto carbon fiber-reinforced polymers (CFRPs) if a Cu interlayer is deposited prior to low-pressure cold spraying. In this present study, Cu was cold sprayed onto CFRP substrates that were coated with either Sn (cold spray) or Ni...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 167-170, May 24–28, 2021,
... in reaction with the surrounding steam environment. Relatively thin oxidation-resistant coatings on Zr-alloy fuel cladding tubes can potentially buy coping time in these off-normal scenarios. In this study, cold spraying, solid-state powder-based materials deposition technology has been developed...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 603-610, May 24–28, 2021,
... as well as heat treatment conditions (maximum temperature, cooling rate, and atmosphere), cold spray of H13 powder went from virtually no deposition to the production of thick dense deposits with a deposition efficiency of 70%. Powder agglomeration, surface state, microstructure evolution, and softening...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 36-43, May 24–28, 2021,
...-pressure CS deposition of NiCoCrAlY and NiCoCrAlYHfSi and discuss the influence of feedstock properties on the deposited BCs. CFD numerical simulation is employed to tailor the spray conditions based on the feedstock characteristics. Secondly, we present the laser assisted cold spray (LACS) deposition...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 153-156, May 24–28, 2021,
... Abstract This study investigates the potential of cold-sprayed tungsten coatings for use in nuclear fusion reactors. Three commercially available tungsten powders were selected from which six series of feedstock were prepared. The feedstocks were deposited on aluminum, steel, and stainless...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 131-138, May 24–28, 2021,
... specimens. Cold sprayed specimens with two different mass concentrations of diamond 20% and 50% in two metallic matrices (Al – lighter than diamond, Cu – heavier than diamond) were compared with the respective pure metal deposits. These pure metal coatings showed rather limited ductility. The diamond...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 157-166, May 24–28, 2021,
... Abstract In previous studies at McGill University, tin was successfully cold sprayed onto carbon fiber reinforced polymers (CFRPs). A “crack-filling” mechanism was described as the deposition mechanism that allowed deposition of tin onto the CFRP. Improving the coating conductivity...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 261-267, May 24–28, 2021,
... into the process, the estimation of such stresses considering the deposition of each layer by numerical methods has not been extensively studied. This work proposes a method for analyzing the evolution of residual stress on a cold spray coating, both on the coating and the substrate, as a function of the deposited...
Proceedings Papers

ITSC2000, Thermal Spray 2000: Proceedings from the International Thermal Spray Conference, 255-262, May 8–11, 2000,
... Abstract Oxygen-free titanium coatings are at present produced using vacuum plasma spray systems. The cold spray process can produce titanium coatings in atmospheric air at reduced cost. Variations of the deposition efficiency as well as the coating characteristics with various process...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 107-114, May 24–28, 2021,
... temperature as well. Deposition efficiency and adhesion and tensile strength measurements were recorded and are used to characterize the hybrid coating process and compare it with traditional techniques. adhesion strength aluminum powder cold spraying deposition efficiency induction heating tensile...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 147-152, May 24–28, 2021,
..., Contribution in Optimization of Zn 151 Cold-Sprayed Coating Dedicated to Corrosion Applications , Surface and Coating Technology, Vol. 400 (2020). doi: 10.1016/j.surfcoat.2020.126193 [12] Y. Ichikawa, R. Tokoro, M. Tanno, and K. Ogawa, Elucidation of Cold-spray Deposition Mechanism by Auger Electron...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 553-560, May 24–28, 2021,
... Abstract The present study compares needed prerequisites for the application of cavitation resistant bronzes by applying different coating techniques, such as cold spraying, HVOF spraying, warm spraying and arc spraying. By optimization to optimum cavitation resistance, the deposited coatings...