ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 561-568, May 24–28, 2021,
... to be more beneficial in terms of wear than massive powders, and graphite was found to be effective for reducing seizure. alumina-reinforced bronze-based composites automotive engine components cold spraying metal-ceramic-lubricant composites microstructure seizure resistance tribological...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 590-595, May 24–28, 2021,
... was applied with a LP-CGS the copper-alumina spraying powder. The coating parameters spraying system to achieve a coating thickness of ~1.5 mm. The can be found in Table 1. coatings were subsequently heat treated to improve the interfacial bond. The produced coatings were examined metallographically regarding...