Proceedings Papers

ITSC1997, Thermal Spray 1997: Proceedings from the United Thermal Spray Conference, 49-54, September 15–18, 1997,
... of the matrix material (Cr203) and solid lubricant (CaF 2 ) is agglomerated, followed by atmospheric plasma spraying (APS) of the agglomerates. Selection of the most appropriate agglomeration and plasma spray parameters as well as the microstructure of the coatings will be discussed. atmospheric plasma...
Proceedings Papers

ITSC1997, Thermal Spray 1997: Proceedings from the United Thermal Spray Conference, 329-333, September 15–18, 1997,
... inflight agglomeration, while the high particle deposition velocities result in the formation of a consolidated coating. We have investigated the production of silicon and silicon carbide coatings using SiCl 4 and CH 4 precursors. Silicon deposits analyzed by transmission electron microscopy were found...
Proceedings Papers

ITSC1996, Thermal Spray 1996: Proceedings from the National Thermal Spray Conference, 107-112, October 7–11, 1996,
... coatings are sprayed with numerous powders made by various processes. These powders include agglomerated sintered powders, fused-crushed powders, extra high carbon WC-Co powders and (W 2 C, WC)-Co powders. After spraying, properties of coatings such as hardness, wear resistance. X-ray diffraction...
Proceedings Papers

ITSC1996, Thermal Spray 1996: Proceedings from the National Thermal Spray Conference, 311-316, October 7–11, 1996,
... to the high oxygen content of commercially available SiC fibers in combination with the elevated process temperatures, the SiC decomposes during plasma spraying. Therefore commercial SiC fibres were coated for temporary oxidation protection with C, TiN or Al 2 O 3 . By different agglomeration techniques using...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 603-610, May 24–28, 2021,
... Abstract A novel powder modification method based on the simultaneous softening and agglomeration of steel powders via heat treatment in a rotary tube furnace has been investigated as a means to improve the cold sprayability of H13 tool steel powder. By adjusting starting powder size and shape...
Proceedings Papers

ITSC1997, Thermal Spray 1997: Proceedings from the United Thermal Spray Conference, 769-774, September 15–18, 1997,
.... A correspondingly lower bond strength was recorded with less coherent coatings generated by agglomerated CHA and SDHA powders. bond strength fracture behavior hydroxyapatite microstructure plasma spraying powder morphology tensile adhesive strength Thermal Spray: A United Forum for Scientific...
Proceedings Papers

ITSC1997, Thermal Spray 1997: Proceedings from the United Thermal Spray Conference, 791-795, September 15–18, 1997,
...-strain curves using the four-point bend tests. The fracture strength values were increased in the order of clad, sintered, agglomerated(no densification), blended and cast & crushed powder coatings. The Co content blended with WC-Co cermet powders significantly increased fracture strain values...
Proceedings Papers

ITSC1997, Thermal Spray 1997: Proceedings from the United Thermal Spray Conference, 909-915, September 15–18, 1997,
... Abstract Agglomerated and sintered TiC-Ni based powders were sprayed by detonation gun spray (DGS) and high-velocity oxy-fuel (HVOF) spray processes. Influence of the binder content (20 and 27 vol.-%) and some alloying elements, such as Mo, Co and N on the coating properties were investigated...
Proceedings Papers

ITSC1998, Thermal Spray 1998: Proceedings from the International Thermal Spray Conference, 379-384, May 25–29, 1998,
... Abstract The present paper describes the synthesis of nanocrystalline 316-stainless steel coatings by high velocity oxy-fuel (HVOF) thermal spraying. The feedstock powders were synthesized by mechanical milling to produce flake-shaped agglomerates with an average grain size of less than 100 nm...
Proceedings Papers

ITSC1996, Thermal Spray 1996: Proceedings from the National Thermal Spray Conference, 97-106, October 7–11, 1996,
... as agglomerated and plasma-densified) of the composition WC-10%Co- 4%Cr have been thoroughly characterized and were sprayed by DCS, HVOF (CDS process) and APS. The microstructures of the coatings were characterized and their wear behaviour was investigated by means of an abrasion wear test. For the best...
Proceedings Papers

ITSC1996, Thermal Spray 1996: Proceedings from the National Thermal Spray Conference, 169-176, October 7–11, 1996,
..., agglomeration with binders, a matter of special interest is the high temperature synthesis of TiC in presence of metallic alloy. The characteristic features of these materials include the carbide phases forming, their bonding with the alloy and reactions during spraying, grain size and their distribution, alloy...
Proceedings Papers

ITSC1996, Thermal Spray 1996: Proceedings from the National Thermal Spray Conference, 349-353, October 7–11, 1996,
... and hardness. A research project presented in this paper dealt with the manufacture of carbon-short-fibre-reinforced aluminum composite coatings by vacuum plasma spraying. The basis of the processing is the agglomeration of aluminum powder and carbon fibres. During the spraying process the aluminum melts...
Proceedings Papers

ITSC1996, Thermal Spray 1996: Proceedings from the National Thermal Spray Conference, 729-734, October 7–11, 1996,
... Abstract Hardmetal-like coatings on the base of titanium carbide as a hard phase and nickel as a metal binder were prepared from agglomerated and sintered powders by plasma spray, detonation gun spray and high-velocity oxygen-fuel spray processes. The powders used in the spray experiments were...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 278-282, May 24–28, 2021,
... modern steel grades such as TWIP (twinning-induced plasticity steel). In this study, a (Ti,Mo)(C,N)-29% Ni hardmetal feedstock powder was prepared by agglomeration and sintering. Coatings were deposited using a high velocity air-fuel (HVAF) spray process. The coating was benchmarked against a standard...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 682-687, May 24–28, 2021,
... that sintered dense powders have a high temperature orthorhombic phase (γ-Li3PO4) that differs from the β-Li3PO4 phase associated with agglomerated Li3PO4. Plasma-sprayed coatings produced from these powders have similarly dense microstructures with fracture-surface morphology like that of sintered bulk...
Proceedings Papers

ITSC2000, Thermal Spray 2000: Proceedings from the International Thermal Spray Conference, 181-186, May 8–11, 2000,
...%. However, the sharp changes in the convergent and divergent nozzle geometry, resulted in fusion and agglomeration of alumina particles leading to spitting during the spraying process. The results clearly showed that alumina coatings of excellent hardness in the range of 920-1290 HV, with a relatively dense...
Proceedings Papers

ITSC2000, Thermal Spray 2000: Proceedings from the International Thermal Spray Conference, 479-486, May 8–11, 2000,
... Abstract Four high velocity thermal spray guns were evaluated in the production of 10%Co-4%Cr tungsten carbide cermets. Three HVOF guns (the JP-5000, JP-5000ST and DJ-2700) and one plasma gun, (the Mettech Axial III) were used to spray the same angular, agglomerated and crushed WC-10Co-4Cr...
Proceedings Papers

ITSC2000, Thermal Spray 2000: Proceedings from the International Thermal Spray Conference, 737-742, May 8–11, 2000,
... and cathode. By decreasing the interactions of the large eddy structures with the formed metal agglomerates one can achieve better control of the particle trajectories and jet divergence. Thus, coatings can be obtained with higher definition and improved reliability. arc behavior high speed photography...
Proceedings Papers

ITSC2000, Thermal Spray 2000: Proceedings from the International Thermal Spray Conference, 843-849, May 8–11, 2000,
..., HVOF, and atmospheric plasma spraying using various forms of feed material, including blended, agglomerated, chemical encased, and attrition-milled powders and filled wires. The investigation involved metallurgical analysis, proving the existence of quasicrystal content and assessing the matrix phase...
Proceedings Papers

ITSC2000, Thermal Spray 2000: Proceedings from the International Thermal Spray Conference, 971-976, May 8–11, 2000,
.... (NEI), respectively. The ability to increase the volume fraction of hard WC phase Metco powder (WC/12Co, 5-45 p.m dia.) consisted of in such a coating, thereby further enhancing its wear solid agglomerates of micron-scale WC and Co particles. resistance. The Nanodyne powder (WC/12Co, 5-30 |j,m dia...