ITSC2000, Thermal Spray 2000: Proceedings from the International Thermal Spray Conference, 463-469, May 8–11, 2000,
... for wear resistant coatings. However, while the production of WC-Co coatings by thermal spray techniques, especially high velocity oxy-fuel flame (HVOF) spraying, is well-established, thermal spraying of TiC-based powders did not lead to satisfactory results so far. This could be attributed...
Proceedings Papers

ITSC 2021, Thermal Spray 2021: Proceedings from the International Thermal Spray Conference, 278-282, May 24–28, 2021,
.... Thermally sprayed coatings based on cubic hard materials such as TiC and TiCN can provide an alternative to widely used Cr3C2-NiCr. While the latter possess a superb oxidation resistance and wear resistance at HT, they are prone to degradation in the presence of Mn, an element commonly alloyed in many...
Proceedings Papers

ITSC2000, Thermal Spray 2000: Proceedings from the International Thermal Spray Conference, 509-514, May 8–11, 2000,
.../asm.cp.itsc2000p0509 Properties of TiC-Ni Based Coatings Deposited by Different HVOF Spraying p. Vuoristo, M. Vaisanen, T. Mantyla Tampere University of Technology, Tampere, Finland L.-M. Berger Fraunhofer Institute for Ceramic Technologies and Sintered t^aterials, Dresden, Germany Hardmetal-like coatings of the TiC...
Proceedings Papers

ITSC1998, Thermal Spray 1998: Proceedings from the International Thermal Spray Conference, 57-61, May 25–29, 1998,
..., 25 -29 May 1998, Nice, France CORROSION RESISTANCE HVOF COATINGS BASED UPON TiC+NiTi AND (Ti,W) C+Ni GUILEMANY J.M., DE PACO J.M., MIGUEL J.R., SANCHEZ J. SMITH P.* Universite of Barcelona, Department of Chemical Engineering and Metallurgy, BARCELONA, SPAIN *London & Scandinavian Metallurgical Co...
Proceedings Papers

ITSC1996, Thermal Spray 1996: Proceedings from the National Thermal Spray Conference, 89-96, October 7–11, 1996,
... on the technology of spray powder preparation, the combination of spray process temperature and particle velocity, and other spray process parameters. It is shown that the TiC-Ni based system can be significantly improved by alloying. This makes the system suitable for coating applications where simultaneous high...
Proceedings Papers

ITSC 2002, Thermal Spray 2002: Proceedings from the International Thermal Spray Conference, 727-732, March 4–6, 2002,
... applications are not suitable for fully describing the technical potential of these composites. TiC-containing layers can complete the range of thermal coating solutions based on tungsten carbide and chromium carbide. The development of TiC-based powders that are better than the prior state of the art...
Proceedings Papers

ITSC 2002, Thermal Spray 2002: Proceedings from the International Thermal Spray Conference, 102-106, March 4–6, 2002,
...Abstract Abstract Nanostructured materials show great potential for a wide variety of technical applications. This paper investigates microstructures and properties of various nanocrystalline TiC-based coatings, which were processed by high velocity oxy-fuel (HVOF) spraying and vacuum plasma...
Proceedings Papers

ITSC1998, Thermal Spray 1998: Proceedings from the International Thermal Spray Conference, 75-82, May 25–29, 1998,
... certain conditions. carbide and titanium oxycarbide that the latter also Recently, much effort has been made to develop forms vacancies in the non-metal and not only in hardmetal-like coatings based on TiC [1-3] and the metal sublattice, metallic titanium also appears as an oxidation product. Cr3C2...
Proceedings Papers

ITSC2000, Thermal Spray 2000: Proceedings from the International Thermal Spray Conference, 515-522, May 8–11, 2000,
... the round, i.e. the particles have not been heated enough during wear properties of TiC-Ni based coatings and found that small the spraying of coating B. powder sizes give improved wear results compared to larger sizes of the same material. 521 Conclusions References 1. HVOF thermal spray powders...
Proceedings Papers

ITSC1996, Thermal Spray 1996: Proceedings from the National Thermal Spray Conference, 729-734, October 7–11, 1996,
... were prepared pected to surpass the performance obtained with conven- from agglomerated and sintered powders by plasma spray, tional hardmetal-like coatings are also of high interest. For detonation gun spray and high-velocity oxygen-fuel spray example, TiC-Ni based coatings are regarded as candidates...
Proceedings Papers

ITSC1997, Thermal Spray 1997: Proceedings from the United Thermal Spray Conference, 909-915, September 15–18, 1997,
...Abstract Abstract Agglomerated and sintered TiC-Ni based powders were sprayed by detonation gun spray (DGS) and high-velocity oxy-fuel (HVOF) spray processes. Influence of the binder content (20 and 27 vol.-%) and some alloying elements, such as Mo, Co and N on the coating properties were...
Proceedings Papers

ITSC 2002, Thermal Spray 2002: Proceedings from the International Thermal Spray Conference, 295-299, March 4–6, 2002,
... behavior and the microhardness. In order to protect the WC-10Co-4Cr powder, this paper evaluates the effectiveness of the addition of a carbon-based material (graphite and amorphous carbon), as attempted by Moreau et Dallaire to protect TiC powders produced by plasma spraying. It discusses the effects...
Proceedings Papers

ITSC2000, Thermal Spray 2000: Proceedings from the International Thermal Spray Conference, 429-434, May 8–11, 2000,
.... TiC-40CrNiMo was sprayed with spray parameters recommended by the Abrasion Wear Test Results. Abrasion wear test results spray gun manufacturer for WC- or Cr3C2- based coatings. are presented in Fig. 9, wear losses are expressed in mm^. According to previous studies TiC-based powders need Due...
Proceedings Papers

ITSC2000, Thermal Spray 2000: Proceedings from the International Thermal Spray Conference, 537-542, May 8–11, 2000,
... based matrices with different content of TiC reinforcing hard particles were sprayed in order to determine wear products abrasive wheels the potential of the coatings for wear and corrosion sucked off hoover arm applications. Composite powder gram size rotating disk 80 wt TiC-Co -63 + 40 ^m 80 wt TiC-Co...
Proceedings Papers

ITSC1997, Thermal Spray 1997: Proceedings from the United Thermal Spray Conference, 131-134, September 15–18, 1997,
...-propagating high (1). That is why the development of competitive metal- temperature mode (SHS). Products were grinded with carbide coatings based on cheap and less harmful Fe/TiC special grinder and ball mill. Plasma spraying in air (APS) material produced by the High Temperature Selt- and in vacuum (VPS...
Proceedings Papers

ITSC 2002, Thermal Spray 2002: Proceedings from the International Thermal Spray Conference, 1029-1032, March 4–6, 2002,
.... FeCr30Mo3+7%graphite+70%TiC: a-x200; b- x1000. Furthermore, the rise of hardness brought by titanium At the same time molybdenum disulfide is more in- carbide increases the resistivity of coating to abrasion. clined to spreading and formation of constant films As regards the inclusions MoS2, CaF2...
Proceedings Papers

ITSC1997, Thermal Spray 1997: Proceedings from the United Thermal Spray Conference, 459-465, September 15–18, 1997,
... coating. Microhardness measurements were conducted on polished cross-sections using a Vickers indentor at 0.5 N for TiC coatings and 0.25 N for Nb coatings. For each sample, ten roughness profiles 32 mm long were analyzed by a SURFASCAN 2D apparatus to determine Ra and Rt. The phase content...
Proceedings Papers

ITSC1996, Thermal Spray 1996: Proceedings from the National Thermal Spray Conference, 169-176, October 7–11, 1996,
... in processing of wear resistant thermal grains size and their distribution, alloys behavior during sprayed coatings, based on titanium carbide. synthesis and spraying. Finally, the abrasive wear and erosion resistance of Al-Si/TiC, Fe-Cr/TiC and Ni-Cr/ Materials and Experimental Procedure TiC coatings...
Proceedings Papers

ITSC1997, Thermal Spray 1997: Proceedings from the United Thermal Spray Conference, 935-942, September 15–18, 1997,
... Advances, C.C. BerndtfEd Published by ASM International, Materials Park, Ohio, USA, 1997 Structure-Property Relationships of TiC-Ni+Ti and (Ti,W) C-Ni Powders Manufactured by the SHS Process, and the Resultant HVOF-Sprayed Coatings J.M. de Paco, J. Nutting, J.M. Guilemany, F.J. Sanchez, J.R. Miguel...
Proceedings Papers

ITSC1998, Thermal Spray 1998: Proceedings from the International Thermal Spray Conference, 1351-1356, May 25–29, 1998,
...Abstract Abstract This paper examines the properties of thermal spray coatings produced by electrothermal explosion. Three refractory carbides (TaC, WC, and TiC) were sprayed onto metal substrates then analyzed using FESEM, EPMA, XRD, and microhardness testing. The new spray technique required...