Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Article Type
Volume Subject Area
Date
Availability
1-1 of 1
Thermoset polyimides
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Proceedings Papers
ITSC 2002, Thermal Spray 2002: Proceedings from the International Thermal Spray Conference, 705-709, March 4–6, 2002,
Abstract
View Papertitled, Development of Functionally Graded Thermal Spray Coatings for Polymer Substrates
View
PDF
for content titled, Development of Functionally Graded Thermal Spray Coatings for Polymer Substrates
In this paper, WC-Co reinforced polymer matrix coatings are sprayed on preheated steel and carbon-fiber reinforced substrates, producing relatively dense, adherent coatings. The particle morphology of the feedstock materials and the microstructure of the HVOF sprayed coatings are characterized and the thermal properties of the polymer powder and coatings are compared. It was found that the deposition and build-up of the polymer coating was only successful when substrates were preheated to the curing temperature of the thermosetting polyimide powder used. Layered coatings of varying polyimide and WC-Co content have been successfully deposited, showing that it is possible to produce graded composite coatings consisting of pure polymer at the substrate and pure WC-Co on the surface. Paper includes a German-language abstract.