ITSC2023, Thermal Spray 2023: Proceedings from the International Thermal Spray Conference, 724-729, May 22–25, 2023,
...) top coatings are used for friction-reduction. As an alternative approach, this study focuses on the possibility of incorporating solid lubricants in self-fluxing alloy coatings. This allows for higher local stress and failure tolerance as well as a reduced process chain. Molybdenum disulfide (MoS 2...
Proceedings Papers

ITSC 2022, Thermal Spray 2022: Proceedings from the International Thermal Spray Conference, 631-636, May 4–6, 2022,
... contain the following alloying elements: The formation of an austenitic microstructure is achieved by nickel (Ni). The addition of chromium (Cr) lead to good corrosion resistance due to formation of an oxide layer. For resistance against pitting corrosion, molybdenum (Mo) can be added. Also, stainless...
Proceedings Papers

ITSC 2022, Thermal Spray 2022: Proceedings from the International Thermal Spray Conference, 736-742, May 4–6, 2022,
... Abstract This paper presents the results of two metals coatings, molybdenum and tantalum, prepared by Controlled Atmosphere Plasma Spray (CAPS) onto Al 6061 substrates that were thermal cycled to calculate the effective coating modulus. Traditional uniaxial tensile testing samples were prepared...
Proceedings Papers

ITSC 2022, Thermal Spray 2022: Proceedings from the International Thermal Spray Conference, 809-814, May 4–6, 2022,
... Abstract The addition of refractory metals represents a promising development approach for future high-entropy alloys (HEAs). Niobium and molybdenum are particularly suitable for increasing hardness as well as wear and corrosion resistance. In the context of surface protection applications...
Proceedings Papers

ITSC 2018, Thermal Spray 2018: Proceedings from the International Thermal Spray Conference, 140-147, May 7–10, 2018,
... Abstract Fatigue crack growth in self-standing plasma sprayed tungsten and molybdenum beams with artificially introduced notches subjected to pure bending was studied. Beams width, thickness and length was 4 mm, 3 mm and 32 mm respectively. Fatigue crack length was measured using...
Proceedings Papers

ITSC 2018, Thermal Spray 2018: Proceedings from the International Thermal Spray Conference, 299-306, May 7–10, 2018,
... Abstract Plasma sprayed zirconium (Zr) metal coatings onto uranium-molybdenum (U-Mo) alloy nuclear reactor fuel foils act as a diffusion barrier between the fuel and the aluminum fuel cladding. Neutron diffraction was performed to investigate the crystallographic phase composition, crystal...
Proceedings Papers

ITSC 2017, Thermal Spray 2017: Proceedings from the International Thermal Spray Conference, 1008-1012, June 7–9, 2017,
... Abstract NiCrBSi is a material generally used in wear-resistant coatings. In order to improve the tribological properties of atmospheric plasma-sprayed NiCrBSi coatings, Molybdenum (Mo) was incorporated into the NiCrBSi coatings to reduce the friction coefficient and wear rate under dry and oil...
Proceedings Papers

ITSC 2017, Thermal Spray 2017: Proceedings from the International Thermal Spray Conference, 394-399, June 7–9, 2017,
... of the components hardfaced with these alloys depends on achieved coating microstructure i.e. on the alloys chemical composition, the coating method and process parameters selected. The present work focuses on iron based hardfacing alloys with varying amount of chromium, vanadium, tungsten, molybdenum, boron...
Proceedings Papers

ITSC 2017, Thermal Spray 2017: Proceedings from the International Thermal Spray Conference, 560-565, June 7–9, 2017,
... Abstract Disk splats are usually observed when the deposition temperature exceeds the transition temperature, whereas thick oxide layer will reduce the adhesion resulting from high deposition temperature. In present study, single molybdenum splats were sprayed onto polished molybdenum...
Proceedings Papers

ITSC 2017, Thermal Spray 2017: Proceedings from the International Thermal Spray Conference, 572-576, June 7–9, 2017,
... of materials having high melting temperatures should be heated to reach a semi-molten or a molten state; 2) oxidation of the metals should be prevented. In this work, the CCDS2000 detonation spray system was used for obtaining molybdenum and tantalum coatings. The coatings were deposited on steel substrates...
Proceedings Papers

ITSC 2015, Thermal Spray 2015: Proceedings from the International Thermal Spray Conference, 460-466, May 11–14, 2015,
... the lamellar interface bonding in metallic coatings has been an important issue which has not been settled effectively. In this study, a shell-core structured powder particle designing with cladding spherical Ni20Cr powders with refractory molybdenum as alloying element is proposed to limit the evaporation...
Proceedings Papers

ITSC 2015, Thermal Spray 2015: Proceedings from the International Thermal Spray Conference, 467-472, May 11–14, 2015,
... and more delta-phase enriched with molybdenum. Another exposure test using a mixed acid of 25%HNO3 and 75%HCl yielded that the δ-Fe was not etched out but the γ-Fe vanished, that is, the δ-Fe of M-SUS has a strong anti-corrosion property. It is considered that the superior corrosion resistance of coating M...
Proceedings Papers

ITSC2014, Thermal Spray 2014: Proceedings from the International Thermal Spray Conference, 31-36, May 21–23, 2014,
... Abstract This study demonstrates the use of bulge testing to evaluate fuel plates for high-performance nuclear reactors. Uranium-molybdenum alloy substrates were plasma sprayed with zirconium and clad between aluminum sheets by hot isostatic pressing. The coated-and-clad samples were cut...
Proceedings Papers

ITSC 2013, Thermal Spray 2013: Proceedings from the International Thermal Spray Conference, 47-50, May 13–15, 2013,
... Abstract The aim of this work is to optimize molybdenum disilicide coatings for high-temperature oxidation protection of metallic surfaces. Agglomerated and sintered MoSi2 powder was deposited on test substrates by atmospheric plasma spraying. The powders and coatings were characterized...
Proceedings Papers

ITSC2012, Thermal Spray 2012: Proceedings from the International Thermal Spray Conference, 7-11, May 21–24, 2012,
... Abstract Molybdenum disilicide (MoSi 2 ) has been applied as protective coating material on various substrates fabricated by different methods due to its good oxidation resistance at elevated temperature, relatively low density and coefficient of thermal expansion and high thermal conductivity...
Proceedings Papers

ITSC2012, Thermal Spray 2012: Proceedings from the International Thermal Spray Conference, 40-46, May 21–24, 2012,
... are reviewed. The bonding formation between particles by controlling deposit surface temperature is essential to form porous deposits. By using flame spraying, different metallic porous deposits up to tens of millimeter thick from refractory molybdenum (Mo) to stainless steel are fabricated with a porosity...
Proceedings Papers

ITSC2012, Thermal Spray 2012: Proceedings from the International Thermal Spray Conference, 70-75, May 21–24, 2012,
... Abstract The future production of low enriched uranium nuclear fuel for test reactors requires a well-adhered diffusion barrier coating of zirconium (Zr) on the uranium/molybdenum (U-Mo) alloy fuel. In this study, the interfacial bond between plasma sprayed Zr coatings and U-Mo fuel has been...
Proceedings Papers

ITSC2012, Thermal Spray 2012: Proceedings from the International Thermal Spray Conference, 87-92, May 21–24, 2012,
... O 3 /Cr 2 O 3 , Al 2 O 3 /TiO 2 and yttria stabilized zirconia (YSZ) were used as coating materials, while molybdenum and silicon carbide served as adhesion-promoting intermediate layers. In order to reduce the residual stresses in the ceramic coatings, specimens with a defined segmented surface...
Proceedings Papers

ITSC2012, Thermal Spray 2012: Proceedings from the International Thermal Spray Conference, 822-827, May 21–24, 2012,
... electrical double layer capacitor electrodes such as carbon. This investigation explored potential of SPPS to deposit molybdenum oxide with microstructures suitable for use as pseudo-capacitive electrodes. It further identified a two-step temperature-programmed heat treatment that resulted in the topotactic...
Proceedings Papers

ITSC2012, Thermal Spray 2012: Proceedings from the International Thermal Spray Conference, 851-857, May 21–24, 2012,
... Abstract In this study, porous molybdenum (Mo) materials were prepared by flame spraying semi-molten particles to low velocity levels. The influence of spray particle state, including particle velocity and melting degree, on microstructure and porosity was investigated to understand...