Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Article Type
Volume Subject Area
Date
Availability
1-1 of 1
O.O. Popoola
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Proceedings Papers
ITSC2000, Thermal Spray 2000: Proceedings from the International Thermal Spray Conference, 905-908, May 8–11, 2000,
Abstract
PDF
Layers of high-purity copper and iron produced by cold gas-dynamic spraying have been thermally processed to induce recrystallization and grain growth. In the case of copper deposits, the as-sprayed structure could be "pinned" by arrays of Cu2O particles present on the surfaces of the feedstock powder, however copper powders of higher purity and sphericity yielded sprayed structures which could be annealed to induce recrystallization and grain growth. The higher purity copper compacts exhibited a morphological change in fracture from a brittle, intraparticle mode in the as-deposited condition, to a ductile, "cup-and-cone" morphology in the annealed condition. For compacts produced from water atomized iron, annealing at sub-critical temperatures produced recrystallization and grain growth as found with copper, and thermal processing in the austenitic region resulted in altogether new and coarser grain structures upon cooling. Ease of thermal processing of cold-sprayed materials may offer additional processing routes for engineered surfaces and functional devices produced in this manner.