Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Article Type
Volume Subject Area
Date
Availability
1-2 of 2
E. Smith
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Proceedings Papers
ITSC1999, Thermal Spray 1999: Proceedings from the United Thermal Spray Conference, 182-184, March 17–19, 1999,
Abstract
PDF
Abstract The use of the wire arc spray process for the production of zinc and aluminum coatings as corrosion protection represents a rapidly growing market. In this paper, the effects of various spray parameters on the performance of the process for these materials are examined. The effects of arc voltage, current, and wire diameter have been studied for their effects on the main factors affecting process performance, spray performance, and application efficiency. The results of this study have led to the development of a spray system or a power supply to maximize the performance of the process for corrosion protection applications. Paper includes a German-language abstract.
Proceedings Papers
ITSC1999, Thermal Spray 1999: Proceedings from the United Thermal Spray Conference, 736-739, March 17–19, 1999,
Abstract
PDF
Abstract In this paper, three goals are attacked, namely synthesis of nanostructured hydroxyapatite (HA) powder, obtaining HA phase constitution close to that of the bone hydroxyapatite, and preserving the initial HA composition and crystal structure in the sprayed coating. HA-aluminum composite coatings are produced using the cold gas dynamic spray method (CGDS). It is observed that the CGDS process enables the application of coatings without changing the phase composition of the HA, whereby the HA biocompatibility is retained. Paper includes a German-language abstract.