Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Article Type
Volume Subject Area
Date
Availability
1-7 of 7
A.J. Allen
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Proceedings Papers
ITSC 2002, Thermal Spray 2002: Proceedings from the International Thermal Spray Conference, 91-95, March 4–6, 2002,
Abstract
PDF
Abstract The pore microstructure of the spray coatings is complicated. However, it can be approximated with three systems, interlamellar pores, intralamellar cracks, and volumetric globular pores. This complex pore morphology can strongly influence the properties of the layer. This paper examines the NiCrAlY layers using the multi-small angle scattering technique to determine the pore system in detail. A model is created based on the analysis of the SEM examinations. The model shows that the inter-lamella system is of the utmost importance. Paper includes a German-language abstract.
Proceedings Papers
ITSC1999, Thermal Spray 1999: Proceedings from the United Thermal Spray Conference, 228-233, March 17–19, 1999,
Abstract
PDF
Abstract This paper describes the technique of anisotropic multiple small-angle neutron scattering (MSANS). Anisotropic MSANS, when combined with anisotropic Porod scattering, electron microscopy, and measurements of elastic modulus and density, has made possible the determination of the porosities, surface areas, mean opening dimensions, mean diameters, and approximate orientation distributions, of the intra-splat cracks and interlamellar pores, as well as the porosity, surface area, and mean diameter, of the globular pores. The changes in these parameters, as a function of annealing, are studied. Paper includes a German-language abstract.
Proceedings Papers
ITSC1999, Thermal Spray 1999: Proceedings from the United Thermal Spray Conference, 799-804, March 17–19, 1999,
Abstract
PDF
Abstract This paper presents novel results of a series of experiments intended to study the role of the size of the feedstock powder on the microstructure of the deposits. For this purpose, Metco and the feedstock powder, yttria-stabilized (8% wt) zirconia, with number-weighted mean particle sizes of 32, 47, 56, and, 88 micrometer, are used. Small-angle neutron scattering and multiple small-angle neutron scattering (MSANS) methods are applied to determine the microstructure of the four deposits. Companion indentation measurements are performed to determine the elastic moduli of the deposits. The paper also discusses the MSANS 3-void model in relation to the anisotropic elastic properties. Paper includes a German-language abstract.
Proceedings Papers
ITSC1998, Thermal Spray 1998: Proceedings from the International Thermal Spray Conference, 1577-1582, May 25–29, 1998,
Abstract
PDF
Abstract The microstructure of plasma-sprayed deposits (PSD) is dominated by two void systems - interlamellar pores and intralamellar cracks - each with a different anisotropy. Varying anisotropics and crack-to-pore ratios within PSDs are responsible for the anisotropic properties observed in the deposits. While it is difficult to apply standard porosity measurement techniques to the assessment of anisotropic microstructures, novel techniques utilizing different approaches have recently emerged. Image analysis (IA) of impregnated PSD samples is the most direct technique. The structure is stabilized by impregnation and then polished and imaged. The limitations of IA lie in the impregnation process and in the subsequent polishing. Also, the images produced from anisotropic materials can be difficult to interpret quantitatively. The technique of small-angle neutron scattering (SANS) has recently been successfully applied to the study of PSDs. The major advantages of SANS are that it does not require sample preparation and that quantitative information can be gotten about the separate crack and pore systems, including their distinctive anisotropics. However, the relationship between the SANS results and the underlying structure is more complex and less intuitive than for IA, and the availability of the SANS technique is limited by the need to have access to a powerful neutron source, such as a reactor. Also, the two techniques present different views of the microstructure because of the different sensitivities in different parts of the size range. This paper compares results from IA and SANS from a set of thick plasma-sprayed ceramic deposits possessing a range of crack/pore microstructures, and discusses how the two techniques might complement one another.
Proceedings Papers
ITSC1998, Thermal Spray 1998: Proceedings from the International Thermal Spray Conference, 1641-1644, May 25–29, 1998,
Abstract
PDF
Abstract The evolution of the void microstructure of yttria-stabilized zirconia (YSZ) plasma-sprayed deposits (PSD) was studied as a function of heating in air from room temperature to 1400°C , and during a constant temperature hold at 1100°C for 19 hours. The samples were studied using the terminal slope (Porod scattering) of small-angle neutron scattering (SANS), modified for the analysis of anisotropic structures. The experiment was done in-situ using a special furnace built for use on the small-angle scattering instrument. SANS Porod scattering can distinguish between the two major void systems - interlamellar pores and intralamellar cracks - that are present in the PSD microstructure. Thus, changes in the void surfaces of the cracks and the pores could be followed separately as a function of temperature. The surface area attributable to the interlamellar cracks significantly decreased at temperatures below 1000°C, whereas the surface area of the interlamellar pores only began to decrease at temperatures above 1000°C. This suggests that there are significant differences in the sintering of these two void systems, probably associated with differences in their sizes and shapes. The first noticeable changes in the void surfaces were observed at temperatures just above 600°C, which is a very low temperature for YSZ. During annealing at 1100°C for 19 hours, there was a decrease in the interlamellar surfaces of about 10%.
Proceedings Papers
ITSC1997, Thermal Spray 1997: Proceedings from the United Thermal Spray Conference, 697-702, September 15–18, 1997,
Abstract
PDF
Abstract The microstructures of as-sprayed and thermally-cycled freestanding and on-substrate deposits of yttria-stabilized zirconia were studied using small-angle neutron scattering (SANS). The SANS analysis allows the interlamellar pores and the intralamellar cracks, which are the two dominant void systems in the microstructure, to be characterized separately. Whereas up to 20% of the void surface area in the as-sprayed deposits was found to be in the cracks, the thermally-cycled deposits contained only a negligible quantity of cracks. At the same time, changes in the pore surface areas between the lamellae (i.e., the interlamellar pores) were much smaller. As a result, the microstructure of the thermally-cycled deposits was much more anisotropic than the microstructure of the as-sprayed deposits. Varying the cooling and the heating rates did not significantly change the microstructure but varying the total time that the deposits were at high temperature did affect the evolution of the surface area. The presence or absence of a bond coat and substrate also did not measurably influence the results.
Proceedings Papers
ITSC1996, Thermal Spray 1996: Proceedings from the National Thermal Spray Conference, 725-728, October 7–11, 1996,
Abstract
PDF
Abstract The porous microstructure of plasma-sprayed deposits prepared from gray-alumina feedstock and from two different yttria-stabilized zirconia (YSZ) feedstocks were studied as a function of spray distance. For each material, the behavior of the two major void systems—intralamellar cracks and interlamellar pores—was investigated. The results offer the first proof that the quantity and the character of the porosity in these materials can be controlled independently by selecting the appropriate processing protocols.