Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Article Type
Volume Subject Area
Date
Availability
1-1 of 1
A. Bahrami
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Proceedings Papers
ITSC2000, Thermal Spray 2000: Proceedings from the International Thermal Spray Conference, 251-254, May 8–11, 2000,
Abstract
PDF
There is typically a large scatter in the observed failure stress, particularly for ceramic coatings. Failure can thus occur not only at the coating-substrate interface where it is desired but also through the coating, the bonding epoxy, or the epoxy/coating interface. A large number of alternative test configurations have been proposed in an attempt avoid such drawbacks, each with their advantages and disadvantages. A test method developed recently by Troczynski and co-workers, known as the Peel Adhesion Test, is of particular interest for this article. The first specimens examined were Ni-WC coatings applied to 150 micrometer thick 1010 stainless steel foils which were grit blasted in the same manner as a bulk substrate would have been. It was observed that the technique appears to offer the capability of providing a sensitive and reproducible measure of the effects of surface treatments and other deposition parameters on coating adhesion.