In this study, we explore the optimization of aerosol deposition parameters to achieve novel TiO2-Fe3O4 graphene oxide composite coatings. Our approach focused on systematically evaluating deposition parameters, including chamber pressure, number of passes, gas flow rate, and sample holder speed, to optimize coating performance.