Abstract
The objective of this study was to quantitatively investigate the build-up of residual stresses in selective laser-melted 316L stainless steel samples and identify the nature of the stresses. In addition, the effectiveness of stress relief heat treatment in reducing residual stresses or changing their characteristics was examined. The results were compared against those obtained from conventionally hot-rolled 316L samples.