This research proposes an experimental methodology towards visually observing high strain rate polymer deformation characteristics at scales relevant to cold spray particle impacts. Macro-scale (~ 3 mm) polymer impact testing via a light gas gun has shown evidence of cold spray indicative features at certain (material, particle/substrate temperature, velocity, etc.) conditions.