Abstract
Thermally sprayed coatings of high performance thermoplastics are of interest especially for the chemical industry for anti-corrosion applications at elevated temperatures. In this paper coatings of polyetherether-keton (PEEK) and polyphenylen-sulphide (PPS) have been produced by simple flamespraying. They have been investigated by optical metallography, FT-IR analysis and DSC-analysis. Among the coating properties also the "in-flight" particles have been studied by wipe-tests and FT-IR analysis in order to assess possible decomposition effects during spraying.