Abstract
This paper provides a short summary of the information that can be found in the literature on the preparation and structure of titanium carbide (TiC) wettable powders. From the work that has been done, it can be concluded that TiC-based coatings can be tailored for applications where complex stress profiles are encountered. Paper includes a German-language abstract.