All solid-state sodium-ion batteries (ASS-SIBs) have great potential for application to large-scale energy storage devices due to their safety advantages by avoiding flammable organics and the abundance of sodium. In this study, plasma spraying was used to deposit Na3Zr2Si2PO12 (NZSP) electrolyte for assembling high performance ASS-SIBs. NZSP electrolyte layers were deposited at different spray conditions using NZSP powders in different particle sizes. The factors influencing the microstructure and compositions of NZSP layers were examined by characterizing the compositions of splat and cross-sectional microstructures of the deposits. It was found that the preferential evaporation loss of Na and P elements occurs severely to result in a large composition deviation from initial powders and spray particle size is key factor which dominates their evaporation loss. The APS NZSP electrolytes present a dense microstructure with well bonded splats which is attributed to low melting point of NZSP. The apparent porosity of the as-sprayed NZSPs was lower than 3 %. The effect of annealing on the microstructure of APS NZSP was also investigated. The performance of typical APS NZSP was also evaluated by assembling an ASS-SIB battery with APS NaxCoO2 (NCO), Na3Zr2Si2PO12 (NZSP) and Li4Ti5O12 (LTO) as cathode, electrolyte and anode, respectively. Results showed that columnar-structured grains with a chemical inter-splat bonding were formed across the interfaces between electrodes and electrolyte. There is no evidence of inter-diffusion of zirconium, cobalt and silicon across the NCO/NZSP interface. With the preliminary battery, the solid electrolyte exhibited an ionic conductivity of 1.21 × 10-4 S cm-1 at 200 oC. The SIB can operate at 2.5 V with a capacity of 10.5 mA h g-1 at current density of 37.4 μA cm-2.

This content is only available as a PDF.
You do not currently have access to this content.