The properties of the coating depend, among other things, on the preparation of the substrate surface and the spray parameters. One of the key properties of the coating is its adhesion to the substrate. Suitable preparation of the substrate surface has a great influence on the adhesion of the thermal spray coating. This work aims to study the influence of surface preparation on roughness of substrate and the resulting surface adhesion of coating. Another aim was to compare the effect of the chosen adhesion measurement method. A series of measurements of the roughness of the samples after grit blasting was performed. The effect of using new and used corundum was also taken into account. The selected coating for testing was TWAS (twin Wire Arc Spray) sprayed Zn15Al. The substrate material was low carbon steel 1.0570. The following adhesion measurement methods were chosen for the experiment - adhesion tensile test according to ASTM C633 - 79 standard, method using a special sample holder based on the ASTM C633 - 79 standard. In addition, a series of measurements were performed using Elcometer 510 Model T.

This content is only available as a PDF.
You do not currently have access to this content.