Sensors to measure gas velocities in high temperature flows need to be robust, low-profile so that they do not obstruct the flow, and easy to apply on metal surfaces. Thermal spray offers a method of making low-cost sensors that can be applied on large areas. Plasma spray was used to deposit an electrically insulating layer of alumina on a 316 stainless steel block. A 17 mm diameter heater coil was deposited on top of the alumina layer by spraying Nichrome from a twin wire arc spray system through a 3D printed polymer mask. A thermocouple junction was built next to the heater by inserting an insulated Constantan wire through a vertical hole drilled in the steel block and spraying steel on the top of the hole to close it and form an electrical connection between the wire and the surrounding substrate. The junction of the wire and the steel formed a thermocouple whose output voltage was calibrated. A flow loop was built to calibrate the sensor by passing air over it at velocities of up to 5 m/s. A series of 2 min long voltage pulses were applied to the heater, increasing its temperature by approximately 5°-10°C each time, before letting it cool. A calibration curve was developed of the air velocity as a function of the time constant for cooling of the sensor.

This content is only available as a PDF.
You do not currently have access to this content.