Spattering is an unavoidable phenomenon in the selective laser melting (SLM) process, which can cause various printing defects and harmful powder recycling. Since the size of powder spattering is too small at the micron level, it is difficult to investigate the entire dynamic spattering process experimentally. The comprehensive understanding of the intricate dynamics of powder spattering during the SLM process remains incomplete. Therefore, we develop a new multiphase flow model to study the transient dynamic behaviors of the gas phase and powder spattering, which agrees well with the experimental observation result. It is the first time that the whole transient dynamic process of powder motion from starting to move induced by the vapor jet to falling to the substrate wall and stopping completely was observed. Powder spattering motion dynamics induced by metal vapor jet and argon gas flow, as a function of time, laser parameters, and location, are presented. The moving speed, total amount, and dropping distribution on the substrate of powder spattering that varies with laser parameters are quantified.

This content is only available as a PDF.
You do not currently have access to this content.