Bond coats are used to protect the superalloy from oxidation and to serve as a bond between the ceramic thermal barrier coating (TBC) layer and the superalloy. During high temperature exposures, a thermally grown oxide (TGO) layer forms between the bond coat and the topcoat due to oxygen diffusion, leading to coating failure in the components. This study aimed to investigate the microstructure evolution of three TBCs with different cold-sprayed bond coat alloys after undergoing isothermal heat treatments. The TBCs were heat treated at 1100 °C for durations of 12, 25, and 50 hours to observe the effects of temperature on the microstructure and phase distribution. The microstructure of heat-treated bond coat alloys was examined using scanning electron microscopy and x-ray diffraction. The findings are discussed in relation to the characteristics of the coating alloy and the application process.