This contribution gives an overview concerning basic principles of cold spraying (CS) and current trends in respective applications. As powder spray technique dealing with solid impacts, cold spraying results in coatings of high purity and unique properties, not attainable by other spray methods. Particularly within the last two decades, cold spraying developed from laboratory scale to a reliable industrial process. The presentation summarizes current models and key parameters in order to achieve and to improve bonding and coating qualities, and gives examples for applications in electronics, mechanical part repair and additive manufacturing.