Abstract
In our laboratory, we have developed a method to simultaneously inject different powders from the central axis direction and radial direction of the cold spray nozzle and are producing a composite coating by this method. In the previous research of our laboratory, an Al-12Si alloy coating with excellent wear resistance was produced by micro-forging assisted cold spray using the simultaneous nozzle injection method of powder in the axial and radial directions. Here, Al- 12Si alloy, which has excellent wear resistance, was used for the coating-formed particles, and stainless steel was used for the micro-forging particles. However, because the micro-forging particles were hollow, they remained in the coating. In this paper, we evaluated the influence of increasing the mixing ratio of micro-forging particles instead of solid (no holes) micro-forging particles on the coating structure. At the same time, the behaviors of particles by computational fluid dynamics are also investigated.