The formation of Nickel coatings on stainless steel substrates and YSZ (Yttria-Stabilized Zirconia) on NiCrAlY in the Atmospheric Plasma Spray (APS) process is investigated. Coating formation over a substrate with an arbitrary shape (an inclined step in this paper) is considered. The topography of the coatings, as well as their microstructure, e.g., porosity, average thickness, and average roughness, are evaluated. An algorithm, which is based on the Monte-Carlo stochastic model, is employed. The significant difference between the coating temperature and that of the substrate leads to the formation of residual thermal stresses. These stresses are analyzed using Object Oriented Finite-element software (OOF) developed by the National Institute of Standards and Technology (NIST). An image of the cross-section of the coating is imported into the code, which utilizes an adaptive meshing technique and Finite- Element Method to calculate residual thermal stresses. The maximum stress in the coatings occurs at the interface between the coating and the substrate. The coatings' topography and microstructure are compared with those of the experiments.

This content is only available as a PDF.
You do not currently have access to this content.