Abstract
Atmospheric plasma spraying (APS) is characterized by complex interactions between input, process and output variables. Process control relies heavily on human expert knowledge and experience. Process diagnostics can provide additional information to the operator and support cognitive processes in task execution. When using non-cascaded torch systems, significant plasma fluctuations occur, affecting the coating quality. High-frequency fluctuations can only be detected by suitable diagnostic systems and interpreted by experienced APS operators. In this study, the state of the plasma jet (area, fluctuation) is investigated depending on total plasma gas flow rate (50 vs. 65 l/min) and the H2 content of plasma gases (17, 20 and 23 vol. %) using high-speed camera pictures. To evaluate plasma fluctuation effects, particle temperature and velocity as well as resulting coating properties (thickness and porosity) are determined for two ceramic systems. The results show that fluctuations of the plasma jet have a significant effect on the particle state and coating quality. The use of a high-speed camera to evaluate the stability of the plasma jet is an attractive method that, when properly integrated, has the potential to provide the human operator with important information to allow rapid assessment of input parameters or the condition of the plasma torch.