Anisotropy of stress-strain behavior, fracture toughness, and fatigue crack growth rate was studied for Inconel 738LC alloy built by the Dynamic Metal Deposition technique (3DMD, a high-speed Directed Energy Deposition technique). The measured quasi-static properties, i.e. stress-strain and fracture toughness showed only subtle anisotropy, with no more than 10% differences found for different orientations. The fatigue crack growth rate was influenced by the specimen orientation more significantly (30% for fatigue crack growth threshold, up to 90% for Paris exponent and coefficient). This pilot study attributes the anisotropy of fatigue crack growth properties to material texture and the columnar grain geometry resulting from directional solidification. The obtained testing results indicate that 3DMD technology can produce materials with good mechanical and fracture properties even from materials considered as non-weldable such as In 738LC. The study provides a solid experimental base for further investigation of the fatigue crack growth mechanism relation to the material texture in 3DMD In 738LC.

This content is only available as a PDF.
You do not currently have access to this content.