There are several challenges when designing components exposed to harsh environments. Cases such as hydraulic turbines and marine propellers are classic examples of demands for materials capable of withstanding erosion and corrosion wear. To enhance and recover worn surfaces, it is usual the use of coatings. This study proposes a new series of coatings based on diffusional effects observed for thermally sprayed chromium carbide coating. A columnar morphology was observed, due to the diffusional gradient perpendicular to the surface. The coating has also shown an absence of porosity and peculiar properties.