Abstract
This study assesses the influence of alumina particle additions on the impact and wear behavior of iron based amorphous coatings. Test results show that the presence of Al2O3 particles improved the impact and wear resistance of the coatings by a factor of three. Deformation and fracture mechanisms under impact loading were also investigated. It was revealed via SEM analysis and finite element simulations that hard second phase particles in the amorphous coating matrix disperse residual stresses generated during impact loading and that brittle particles absorb impact energy by fracturing, which plays a vital role in crack prevention and arresting. Abstract only; no full-text paper available.