Abstract
In this work, two agglomerated hydroxyapatite (HA) powders, with and without heat treatment, were cold sprayed using various spraying parameters on metallic (Ti-6Al-4V) and polymeric (PVA) substrates. The structure of the agglomerated powders and corresponding features of the coatings were examined. For both types of substrates, it was shown that submicron HA powders produce homogenous layers with submicron HA grains. In the case of non-heat treated particles, thick layers could be obtained due to the binding action of residual by-products. HA layers were also found to be adherent after immersion in water, which could potentially lead to the fabrication of ceramic coated hydrogels.