This study demonstrates the feasibility of an in-situ heat treatment for cold spray coatings. By controlling heat flow, temperature gradients are maintained in the coatings, leading to the development of graded mechanical properties. Initial experimental results validate both the starting idea and the first results of numerical simulations.