This study evaluates the friction and wear behavior of iron-base coatings produced by arc spraying using experimental cored wires. Coating microstructure was analyzed and various wear tests were performed. The results show that the tribological properties of the ferrous coating materials are greatly affected by porosity, oxide inclusions, particle shape, and microhardness.