Abstract
The aim of this study is to evaluate the microstructure and corrosion properties of Fe-based coatings produced using different HVAF spray guns. Differences in microstructure, phase composition, porosity, oxide content, and corrosion behavior were observed among the coatings depending on the gun and spraying parameters. The results are presented and discussed in detail.