Nanostructured zirconia coatings were prepared by solution plasma spraying. The phase composition and microstructure of the coatings and powders dried from solution were observed by XRD and SEM. Fine grained nanostructured zirconia coatings can be obtained. Nano-zirconia coatings adhered well with the substrate, and exhibited few vertical cracks.