Abstract
Yttria-stabilized zirconia (YSZ) coatings have been frequently used as a thermal protective layer on the metal or alloy component surfaces. In the present study, ZrO2-7%Y2O3 thermal barrier coatings (TBCs) were successfully deposited by DC (direct current) plasma spray process under very low pressure condition (less than 1 mbar) using low-energy plasma guns F4-VB and F100. The experiments were performed to evaluate the thermal shock resistance of the different TBC specimens which were heated to 1373 K at a high-temperature cycling furnace and held for 0.5 h, followed by air cooling under room temperature during 0.2 h. For comparison, the corresponding APS counterparts were also elaborated to carry out the similar experiments. The results indicated that the VLPPS coatings displayed better thermal shock resistance. Moreover, the failure mechanism of the coatings was also elucidated.