Abstract
Complexity in dynamics and mechanism of supersonic flame formation and effects of processing variables has made the understanding of interaction of particles and flame a difficult task. Lack of such understanding limits the possibilities of controlling the process to obtain desired in-flight particles temperature and velocity and consequent particles state. This problem is even more pronounced in TS systems with no dedicated decoupled temperature and velocity controlled regime. Different approaches based on total volume flow, back pressure and fuel to oxygen ratio have been examined to address the robustness of each approach to control the temperature and velocity. WC-CoCr material was used employing DJ-2600 torch. A guideline to control the in-flight particles temperature and velocity based on process variables is provided. A process map was developed to establish a correlation between process, in-flight particles state, microstructure, properties and performance.