Metallic coatings as protection against extraordinary attack of mechanical wear mechanisms such as welded layers or sintered coatings are wordwide standardized. There exists a lot of empirical knowledge, but no exact method is known to foresee the grade of wear in dependance of all important influences in tribological systems. Paper text in German.