Abstract
After a short description of the rod flame spray method some european products of rod flame spray guns will shown. Some properties of the most used layers of oxide ceramic materials will be introduced. Several applications shows the versatility of this technique. Paper text in German.
This content is only available as a PDF.
Copyright © 1999 Verlag für Schweißen und verwandte Verfahren DVS-Verlag GmbH. All rights reserved.
1999
ASM International
Issue Section:
Poster Session: Applications and Case Studies