Abstract
Coatings with magnetic properties were produced by vaccum plasma spraying of different Nd-Fe-B powders onto stainless¬steel substrates. Microscopic examination of the coatings in a light microscope revealed a low porosity and a good bonding to the substrate. Scanning electron microscope examinations have shown different phases in these coatings. The magnetic properties of the coatings are also presented. Paper text in German.