Abstract
Plasma transferred arc (PTA) allows to weld a metallic coating to a metal substrate in order to improve their wear and corrosion resistance. This process is mainly used for steel reclamation and the principal applications are coatings of valves, valve seats in automotive industry and extruder screws for plastic industry. This paper describes the tape casting of NiCu and NiCoCrAlTaY particles on Ni-based alloys and the various organic additives used in addition to a homogeneous metallic film. The initial results of treating these films with PTA regeneration are described. Paper includes a German-language abstract.