Deformation stages and specific features were studied by mesomechanical methods under tension of plasma sprayed coating-steel matrix composites. The effect of coating quality on the deformation of the matrix at the mesolevel was revealed. The results obtained make it possible to predict reliability and durability of this kind of coating and of the entire composite.