For the purpose of getting high hardness and high wear-resistant coating by arc spraying technology, the arc spraying of 7Cr13 cored wire is adopted in this paper. The metallurgical process of the cored wire arc spraying is discussed. The bond strength, hardness and tribological properties of the composite coating are investigated.