Abstract

The use of overdriven detonation waves can promote coating fabrication from powder materials with high melting temperature and improve the quality coating for all materials. The detonation products flow behind overdriven detonation has kinetic and thermal energy values significantly exceeding those for self-sustaining Chapman- Jouguet's detonation, conventionally used for detonation spraying. This makes it possible to design a micro-gun and, as a consequence, the equipment for internal surface coating.